No one wants defective metal castings. Learn how to identify and prevent 6 common porosity defects! 

  1. Surface Porosity
  2. Reaction Porosity
  3. Gas Hole Porosity
  4. Oxide Inclusions
  5. Shrinkage Porosity
  6. Hydrogen Gas Porosity

Thank you to our special guests at Porosity Solutions: https://porositysolutions.com/

  • Brad Hohenstein - Porosity Solutions Founder
  • Ernie Coberly - Porosity Solutions Instructor

And your friends at Batesville Products: https://batesvilleproducts.com/

  • Monty Fullerton - Manufacturing Engineer (guest)
  • Tim Williams - National Sales Manager (host)
  • Rachel Weber - Regional Sales Consultant (moderator)
  • Johnathan Johnson - Regional Sales Consultant (moderator)

CHAPTERS

00:00 - 00:39 Intro

00:39 - 02:15 Welcome Guests

02:15 - 03:34 Surface Porosity

03:34 - 04:55 Reaction Porosity

04:55 - 06:52 Gas Hole Porosity

06:52 - 08:53 Oxide Inclusions

08:53 - 11:42 Shrinkage

11:42 - 16:39 Hydrogen Gas Porosity

16:39 - 17:13 Outro